Physical properties
Loss Tangent at 10GHz: ~5 x 10-4 @ 300K, ~3 x 10-4 @ 77K; Thermal expansion: 10.4 (x 10-6/°C)
Physical form
cubic (a = 3.905 Ã…)
Molecular Weight: 183.49. Empirical Formula: O3SrTi. linearFormula: SrTiO3. Quality Level: 100. form: crystalline (cubic (a: 3.905 Å)). dielectric constant: ~300. hardness: 6 (, Mohs). reaction suitability: reagent type: catalystcore: titanium. size: 10 . mm × 10 . mm × 0.5 . mm . mp: 2060 . °C (lit.), 2080 . °C. density: 4.81 . g/mL . at 25 . °C (lit.), 5.175 . g/mL . at 25 . °C. semiconductor properties: <. 100>. . SMILES string: [Sr++].[O-][Ti]([O-]): O. InChI: 1S/3O.Sr.Ti/q. 2*-1. +2. . InChI key: VEALVRVVWBQVSL-UHFFFAOYSA-N. Storage Class Code: 11 - Combustible Solids. WGK: WGK 3. Flash Point(F): Not applicable. Flash Point(C): Not applicable. Personal Protective Equipment: Eyeshields, Gloves, type N95 (US).
- UPC:
- 12141504
- Condition:
- New
- HazmatClass:
- No
- MPN:
- 634689-1EA
- CAS:
- 12060-59-2