General description
Nickel electroplating solution is designed for the fabrication of low stress, smooth and pinhole-free nickel films.
Features and Benefits
- Deposits have low internal stress and are very ductile.
- Surfaces are uniform and smooth with well-controlled thickness and excellent uniformity.
- As plated Ni films have small grains in the range of 10 - 50 nm. Grain size orientations are (111) and (200) for FCC (face centred cubic).
- Qualified bath metrology for replenishment and a long shelf life.
Electroplated Ni film (5-10 μm thickness) properties:
- Density: 8.1 g/cm3
- Young′s modulus: 210 GPa
- Internal stress 33 ± 13 MPa
- Tensile strength: 585 ± 40 MPa
- Grain size: 10-50 nm
form: liquid. contains: 1.25 . g/L±0.125 . g/L stabilizer, 0.015 . g/L±0.0015 . g/L wetting agent, 4.25 . g/L±0.25 . g/L Stress reducer. composition: 30 g/L ±. 0.5 g/L H
3BO
3 , 170g/L ±. 5 g/L Ni(SO
3NH
2)
2.4H
2O , 9.51 g/L ±. 1 g/L NiBr
2 .xH
2O . Pictograms: GHS05,GHS08,GHS09. Signal Word: Danger. Hazard Statements: H317 - H318 - H334 - H341 - H350 - H360FD - H372 - H410. Precautionary Statements: P202 - P273 - P280 - P302 + P352 - P305 + P351 + P338 - P308 + P313. Hazard Classifications: Aquatic Acute 1 - Aquatic Chronic 2 - Carc. 1B - Eye Dam. 1 - Muta. 2 - Repr. 1B - Resp. Sens. 1 - Skin Sens. 1 - STOT RE 1. Storage Class Code: 6.1D - Non-combustible, acute toxic Cat.3 / toxic hazardous materials or hazardous materials causing chronic effects. WGK: WGK 3. Flash Point(F): Not applicable. Flash Point(C): Not applicable.